Boiler Tube

ASTM A210 Seamless Boiler Tube

ASTM A210 Grade C Seamless Boiler and Superheater Tubes sizes and thicknesses usually furnished to this specification are 1/2 in. to 5 in. [12.7 to 127 mm] in outside diameter and 0.035 to in. 0.500 [0.9 to 12.7 mm], inclusive, in minimum wall thickness.

SA-210C is ASME standard steel grade, which is medium carbon steel pipe for boiler and superheater pipe, pearlescent hot strong steel.

Applicable conditions: widely used in 300MW, 600MW and other large capacity power station boilers, heating surface piping and header, steam water piping, etc. with working temperature lower than 500 ℃, such as water wall, economizer, low-temperature superheater, etc.

Manufacture: Seamless process ,Hot-finished or Cold-finished
Wall thickness(WT): 0.9 mm——12.7 mm.
Outer diameter (OD): 12.7 mm——127 mm
Length: 6M or specified length as required.
Ends: Plain End, Beveled End, Threaded

ASTM A210 Grade C Seamless Boiler and Superheater Tubes

OD (mm)Wall Thickness(mm)
 22.533.544.5566.5-77.5-88.5-99.5-101112
Φ25-Φ28        
Φ32        
Φ34-Φ36        
Φ38        
Φ40         
Φ42         
Φ45        
Φ48-Φ60       
Φ63.5       
Φ68-Φ73        
Φ76    
Φ80    
Φ83    
Φ89    
Φ95    
Φ102    
Φ108    
Φ114     
Φ121     
Φ127     

Heat Treatment
Hot-finished tubes need not be heat treated.
Cold- finished tubes shall be given a subcritical anneal, a full anneal, or a normalizing heat treatment after the final cold finishing process.

Chemical Composition Of ASTM A210 Grade C

ASTM A210Gradechemical composition:
C(a)SiMnPS
C≤0.35≥0.100.29-1.06≤0.035≤0.035

Mechanical  Properties Of ASTM A210 Grade C

Mechanical  PropertiesGrade C
  Tensile strength, min, ksi [MPa]70 [485]
  Yield strength, min, ksi [MPa]40 [275]
  Elongation %30
  HRB89
  HB179

Note:Mechanical property requirements do not apply to tubing smaller than 1/8 in.

Tolerances of  Wall Thickness

Outside
Diameter,
in. [mm]
Wall Thickness, %
0.095[2.4] and UnderOver 0.095 to 0.150
[2.4 to 3.8], incl
Over 0.150 to 0.180
[3.8 to 4.6], incl
Over 0.180,[4.6]
OverUnderOverUnderOverUnderOverUnder
Seamless, Hot-Finished Tubes
4 [101.6] and under400350330280
Over4[101.6]….….350330280
Seamless, Cold-Finished Tubes
 OverUnder
1 1 ⁄ 2 [38.1] and under200
Over 1 1 ⁄ 2 [38.1]220

Tolerances of  Outside Diameter

Outside Diameter,in. [mm]Permissible Variations, in. [mm]
OverUnder
Hot-Finished Seamless Tubes
4 [101.6] and under1 ⁄ 64 [0.4]1 ⁄ 32 [0.8]
Over 4 to 7 1 ⁄ 2 [101.6 to 190.5], incl1 ⁄ 64 [0.4]3 ⁄ 64 [1.2]
Over 7 1 ⁄ 2 to 9 [190.5 to 228.6], incl1 ⁄ 64 [0.4]1 ⁄ 16 [1.6]
Cold-Finished Seamless Tubes
Under 1 [25.4]0.004 [0.1]0.004 [0.1]
1 to 1 1 ⁄ 2 [25.4 to 38.1], incl0.006 [0.15]0.006 [0.15]
Over 1 1 ⁄ 2 to 2 [38.1 to 50.8], excl0.008 [0.2]0.008 [0.2]
2 to 2 1 ⁄ 2 [50.8 to 63.5], excl0.010 [0.25]0.010 [0.25]
2 1 ⁄ 2 to 3 [63.5 to 76.2], excl0.012 [0.3]0.012 [0.3]
3 to 4 [76.2 to 101.6], incl0.015 [0.38]0.015 [0.38]
Over 4 to 7 1 ⁄ 2 [101.6 to 190.5], incl0.015 [0.38]0.025 [0.64]
Over 7 1 ⁄ 2 to 9 [190.5 to 228.6], incl0.015 [0.38]0.045 [1.14]

 Tolerances of Length

Method of
Manufacture
Outside
Diameter,
in. [mm]
Cut Length,in. [mm]
OverUnder
Seamless, hot-finishedAll sizes3 ⁄ 16 [5]0 [0]
Seamless, cold-finishedUnder 2 [50.8]1 ⁄ 8 [3]0 [0]
2 [50.8] and over3 ⁄ 16 [5]0 [0]
2 [50.8] and over3 ⁄ 16 [5]0 [0]

 Mechanical Tests Required
(1)Tension Test—One tension test shall be made on a specimen for lots of not more than 50 tubes. Tension tests shall be made on specimens from two tubes for lots of more than 50 tubes .
(2)Flattening Test—One flattening test shall be made on specimens from each end of one finished tube from each lot.
(3)Flaring Test—One flaring test shall be made on speci- mens from each end of the one finished tube from each lot.
(4)Hardness Test—Brinell or Rockwell hardness tests shall be made on specimens from two tubes from each lot .
(5)Hydrostatic or Nondestructive Electric Test—Each tube shall be subjected to the hydrostatic,

ASTM A210 Grade A1 Seamless Boiler and Superheater Tubes sizes and thicknesses usually furnished to this specification are 1/2 in. to 5 in. [12.7 to 127 mm] in outside diameter and 0.035 to in. 0.500 [0.9 to 12.7 mm], inclusive, in minimum wall thickness.

Manufacture: Seamless process ,Hot-finished or Cold-finished
Wall thickness(WT): 0.9 mm——12.7 mm.
Outer diameter (OD): 12.7 mm——127 mm
Length: 6M or specified length as required.
Ends: Plain End, Beveled End, Threaded

ASTM A210 Grade A1 Seamless Boiler and Superheater Tubes

OD (mm)Wall Thickness(mm)
 22.533.544.5566.5-77.5-88.5-99.5-101112
Φ25-Φ28        
Φ32        
Φ34-Φ36        
Φ38        
Φ40         
Φ42         
Φ45        
Φ48-Φ60       
Φ63.5       
Φ68-Φ73        
Φ76    
Φ80    
Φ83    
Φ89    
Φ95    
Φ102    
Φ108    
Φ114     
Φ121     
Φ127     

Manufacture
ASTM A210 Grade A1 Seamless boiler tubes are made by the seamless process and are either hot-finished or cold-finished, as specified.

Heat Treatment
Hot-finished tubes need not be heat treated.
Cold- finished tubes shall be given a subcritical anneal, a full anneal, or a normalizing heat treatment after the final cold finishing process.

Chemical Composition Of ASTM A210 Grade A1

StandardGradechemical composition:
C(a)SiMnPS
ASTM A210A-1≤0.27≥0.10≤0.93≤0.035≤0.035

Mechanical  Properties Of ASTM A210 Grade A1

Mechanical  PropertiesGrade A-1
  Tensile strength, min, ksi [MPa]60 [415]
  Yield strength, min, ksi [MPa]37 [255]
  Elongation %30
  HRB79
  HB143

Note:Mechanical property requirements do not apply to tubing smaller than 1/8 in.

The dimensional tolerances of ASTM A210 Seamless Medium-Carbon Steel Boiler and Superheater Tubes

Tolerances of  Wall Thickness

Outside
Diameter,
in. [mm]
Wall Thickness, %
0.095[2.4] and UnderOver 0.095 to 0.150
[2.4 to 3.8], incl
Over 0.150 to 0.180
[3.8 to 4.6], incl
Over 0.180,[4.6]
OverUnderOverUnderOverUnderOverUnder
Seamless, Hot-Finished Tubes
4 [101.6] and under400350330280
Over4 [101.6]….….350330280
Seamless, Cold-Finished Tubes
 OverUnder
1 1 ⁄ 2 [38.1] and under200
Over 1 1 ⁄ 2 [38.1]220

 
Tolerances of  Outside Diameter

Outside Diameter,in. [mm]Permissible Variations, in. [mm]
OverUnder
Hot-Finished Seamless Tubes
4 [101.6] and under1 ⁄ 64 [0.4]1 ⁄ 32 [0.8]
Over 4 to 7 1 ⁄ 2 [101.6 to 190.5], incl1 ⁄ 64 [0.4]3 ⁄ 64 [1.2]
Over 7 1 ⁄ 2 to 9 [190.5 to 228.6], incl1 ⁄ 64 [0.4]1 ⁄ 16 [1.6]
Cold-Finished Seamless Tubes
Under 1 [25.4]0.004 [0.1]0.004 [0.1]
1 to 1 1 ⁄ 2 [25.4 to 38.1], incl0.006 [0.15]0.006 [0.15]
Over 1 1 ⁄ 2 to 2 [38.1 to 50.8], excl0.008 [0.2]0.008 [0.2]
2 to 2 1 ⁄ 2 [50.8 to 63.5], excl0.010 [0.25]0.010 [0.25]
2 1 ⁄ 2 to 3 [63.5 to 76.2], excl0.012 [0.3]0.012 [0.3]
3 to 4 [76.2 to 101.6], incl0.015 [0.38]0.015 [0.38]
Over 4 to 7 1 ⁄ 2 [101.6 to 190.5], incl0.015 [0.38]0.025 [0.64]
Over 7 1 ⁄ 2 to 9 [190.5 to 228.6], incl0.015 [0.38]0.045 [1.14]

Tolerances of Length

Method of
Manufacture
Outside
Diameter,
in. [mm]
Cut Length,in. [mm]
OverUnder
Seamless, hot-finishedAll sizes3 ⁄ 16 [5]0 [0]
Seamless, cold-finishedUnder 2 [50.8]1 ⁄ 8 [3]0 [0]
2 [50.8] and over3 ⁄ 16 [5]0 [0]
2 [50.8] and over3 ⁄ 16 [5]0 [0]

Mechanical Tests Required
(1)Tension Test—One tension test shall be made on a specimen for lots of not more than 50 tubes. Tension tests shall be made on specimens from two tubes for lots of more than 50 tubes .
(2)Flattening Test—One flattening test shall be made on specimens from each end of one finished tube from each lot.
(3)Flaring Test—One flaring test shall be made on speci- mens from each end of the one finished tube from each lot.
(4)Hardness Test—Brinell or Rockwell hardness tests shall be made on specimens from two tubes from each lot .
(5)Hydrostatic or Nondestructive Electric Test—Each tube shall be subjected to the hydrostatic,

ASTM A210 Grade A1 Seamless Boiler Tubes Marking
In addition to the marking prescribed in Specification A 450/A 450M, the marking shall indicate whether the tube is hot-finished or cold-finished.

Surface Condition
If pickling or shot blasting or both are required, this shall be specifically stated in the order.